Re: Dried up
Posted: Sat Sep 24, 2016 5:19 am
Just a thought.
I have a small ultrasonic cleaner left from when I was doing jewelry, and decided to give it a try.
I put some h2o in three bottles and fired that sucker up.
After about 1 hour the paint in the bottles had all reconstituted itself.
NOW, for the TE pens.
I unscrewed the tip and put some h2o in and put them in with the Glassline paints, and Viola,. the same thing.
I just saved about $400.00 for nothing.
NOTE VERY IMPORTANT. My TE pens were about 10 years old, so this might not be applicable now.
The threads are LEFT HANDED!!!!
I have a small ultrasonic cleaner left from when I was doing jewelry, and decided to give it a try.
I put some h2o in three bottles and fired that sucker up.
After about 1 hour the paint in the bottles had all reconstituted itself.
NOW, for the TE pens.
I unscrewed the tip and put some h2o in and put them in with the Glassline paints, and Viola,. the same thing.
I just saved about $400.00 for nothing.
NOTE VERY IMPORTANT. My TE pens were about 10 years old, so this might not be applicable now.
The threads are LEFT HANDED!!!!