Hi all...have printer...have images...have applied to glass and allowed to dry...now temps & soak times...20 minutes seems a LONG time to soak at 1375 when I only ever soak for 8-10mins with enamels....your thoughts???
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: lettering fused into or onto glass
I haven't done a lot of experimenting with decals but my thoughts would be, "well it's only about 10 minutes extra, and there's some plasticky-type stuff that has to burn off, so I guess it makes sense."
Re: lettering fused into or onto glass
eeeppp...I don't want to wreck the kilnload, but I want to fire them up and see
(I know someone is ging to suggest a test firing...but I am impatient *sigh* not a good trait in a glass artist I know)
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: lettering fused into or onto glass
In my experience, extending a soak 12 minutes at 1375 would be insignificant in any negative way.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: lettering fused into or onto glass
your opinions...is 1375 for 20 mins long enough to fire polish the glass too...trying to skip a firing

Re: lettering fused into or onto glass
ANYONE??? lol 
Re: lettering fused into or onto glass
Maybe. LOOK!
Re: lettering fused into or onto glass
CJ--you might want to try a scrap piece first, let us know!