Mistakes and Taking Risks
Moderator: Brad Walker
-
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Mistakes and Taking Risks

Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Mistakes and Taking Risks
Not sure if this link will work but try this: https://www.facebook.com/uroborosglass? ... n=timeline
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
- Posts: 37
- Joined: Tue May 09, 2006 8:28 am
- Location: israel
- Contact:
-
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Mistakes and Taking Risks
What a wonderful time in Portland. I love it there sooo much. Got to go out to dinner with some wonderful people and met Carol Reynolds who is working tirelessly along with Kat and Kathy to make some great new changes at Uroboros. Everyone is so kind that it is just such a pleasure to create in the large kilns. I did not get a chance to slump my large vessel form though as I wanted to put one of the panels back in to make it slightly different. Perhaps easier for the staff at Uroboros though as they would have had to put bricks all around the big Euclid Kiln to make it taller and it was a weekend and well, just better to make it easier on everyone to just refire. AND I am glad I did as the piece turned out better than the first time. Yeah!! Les
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Mistakes and Taking Risks
The 3rd photo is of the piece I put back in the kiln to hide some of the white and it turned out much better but at least you can see it .
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Mistakes and Taking Risks
I also made a new colour bar their tooo and just sliced into it at home here. There was no saw available down at the factory so I had to waite, and now I have some nice mountain and water colours to play with again. Yeah again. Les
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Mistakes and Taking Risks
http://www.canadahouse.com/dynamic/artw ... rkID=33410
Well finally the journey has ended and pieces are at the gallery and hopefully will find a lovely home. Such a great experience and the Uroboros people are totally wonderful and supportive and kind |( and fun toooo! )
Leslie
Well finally the journey has ended and pieces are at the gallery and hopefully will find a lovely home. Such a great experience and the Uroboros people are totally wonderful and supportive and kind |( and fun toooo! )
Leslie