Help with new project
Posted: Sun May 25, 2003 10:39 am
Hi everyone
I´just beginning a new project - very good money - that is a lot of sinks...
I read all that I could find in the archives, but still have lots of doubts. Barbara Cashman is helping me , but I have some questions that I´m sure some of you can help me.
The person that asked me for the sinks wants me to be her exclusive one doing them, and of course, it will be very good
I will work with float glass, and I´m planning to do two tests: one using two layers of 3/8 in so that I can use paint and/or use some inclusions. The other with a piece of 3/4 in.
I´ll try drop ring and molds, so I can find witch one works better for me.
What would be a good schedule for full fuse and for tack fuse of these glasses?
I could´n buy Grahams book yet, and the others I have are not very specific about float...
Please, any help about the schedule, and/or about sinks will be very ,very good.
Thanks a lot for your time
Luiza
I´just beginning a new project - very good money - that is a lot of sinks...
I read all that I could find in the archives, but still have lots of doubts. Barbara Cashman is helping me , but I have some questions that I´m sure some of you can help me.
The person that asked me for the sinks wants me to be her exclusive one doing them, and of course, it will be very good

I will work with float glass, and I´m planning to do two tests: one using two layers of 3/8 in so that I can use paint and/or use some inclusions. The other with a piece of 3/4 in.
I´ll try drop ring and molds, so I can find witch one works better for me.
What would be a good schedule for full fuse and for tack fuse of these glasses?
I could´n buy Grahams book yet, and the others I have are not very specific about float...
Please, any help about the schedule, and/or about sinks will be very ,very good.
Thanks a lot for your time
Luiza