question RE: Full Fusing

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Larry
Posts: 4
Joined: Wed May 07, 2003 9:57 pm

question RE: Full Fusing

Post by Larry »

i used a black base layer with red and gray frit on the design layer with some noodles and stringers too. when i opened the kiln only the stringers and noodles were visible. i used decent quantity of the frit. what happened?
Dani
Posts: 493
Joined: Mon Mar 10, 2003 3:17 pm
Contact:

Post by Dani »

Opas or cathedrals on which items? Was your base glass an opalescent and your frit a cathedral?.... you won't get very dramatic results that way... except for a disappearing act.
Post Reply