Has anyone heard of PC-7 two part epoxy? And if so, where it can be purchased? It was recommended to me as a very strong glue for glass wall hangings.
Thanks for you help!
Katy
PC-7 two part epoxy
Moderators: Brad Walker, Tony Smith
-
Katy Mattice
- Posts: 6
- Joined: Sun Mar 09, 2003 9:00 pm
- Location: Florida and Wisconsin
PC-7 two part epoxy
K.Mattice
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: PC-7 two part epoxy
PC 7 is an incredibly strong epoxy. I have bought it at the neighborhood hardware store. It is not a pretty color if that is an issue for you.Katy Mattice wrote:Has anyone heard of PC-7 two part epoxy? And if so, where it can be purchased? It was recommended to me as a very strong glue for glass wall hangings.
Thanks for you help!
Katy
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Katy Mattice
- Posts: 6
- Joined: Sun Mar 09, 2003 9:00 pm
- Location: Florida and Wisconsin
PC-7 two part epoxy
Hi Bert,
Thanks for the info...I may just try and find it, as color is not a concern on this piece.
Katy
Thanks for the info...I may just try and find it, as color is not a concern on this piece.
Katy
K.Mattice