Page 1 of 1
PC-7 two part epoxy
Posted: Wed May 28, 2003 8:29 pm
by Katy Mattice
Has anyone heard of PC-7 two part epoxy? And if so, where it can be purchased? It was recommended to me as a very strong glue for glass wall hangings.
Thanks for you help!
Katy
Re: PC-7 two part epoxy
Posted: Wed May 28, 2003 10:02 pm
by Bert Weiss
Katy Mattice wrote:Has anyone heard of PC-7 two part epoxy? And if so, where it can be purchased? It was recommended to me as a very strong glue for glass wall hangings.
Thanks for you help!
Katy
PC 7 is an incredibly strong epoxy. I have bought it at the neighborhood hardware store. It is not a pretty color if that is an issue for you.
PC-7 two part epoxy
Posted: Thu May 29, 2003 9:31 am
by Katy Mattice
Hi Bert,
Thanks for the info...I may just try and find it, as color is not a concern on this piece.
Katy