Will a 70 grit diamond belt will "eat" glass significantly faster than a typical Glastar-type grinder?
I grind lots of small pieces to shape and I'm looking to speed things up.
Thanks,
Paul
Grinder vs. Diamond Belt
Moderators: Brad Walker, Tony Smith
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
-
Jackie Beckman
- Posts: 475
- Joined: Sun Mar 09, 2003 5:01 pm
- Location: Arizona
- Contact:
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
-
Jackie Beckman
- Posts: 475
- Joined: Sun Mar 09, 2003 5:01 pm
- Location: Arizona
- Contact:
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Grinder vs. Diamond Belt
We use a very rough diomond grinding wheel 30 / 40Paul Tarlow wrote:Will a 70 grit diamond belt will "eat" glass significantly faster than a typical Glastar-type grinder?
I grind lots of small pieces to shape and I'm looking to speed things up.
Thanks,
Paul
Then a 40 / 50 for finer
Electro plated
We use a bed 2 grind on n tip it twisal the glass arround
Or we also ajust the height
We then get a multy beviled edge we then finish this off by hand then
Tumble finish em then polish up the one or 2 surfaces
Thats how we do the pebbles