Firing Schedule for Hanovia Mother of Pearl Luster
Moderators: Brad Walker, Tony Smith
Firing Schedule for Hanovia Mother of Pearl Luster
Does anyone have a firing schedule for hanovia mother of pearl luster? Last night I tried it out - I took it up to 1310, held for ten minutes. Unfortunately, what I ended up with is an etched look - definately not mother of pearl. I think I probably took it too high and it burned off. Anyone else ever use the stuff? Thx.
-
Cynthia
http://clayartcenter.com/glaze_hanova.htm
I think it's cone 018-019. Call your ceramics folks for a conversion if you need one since I don't know what temp that is. Info about all hanovia products and firing cones are at the above link.
I think it's cone 018-019. Call your ceramics folks for a conversion if you need one since I don't know what temp that is. Info about all hanovia products and firing cones are at the above link.
cone 018 to 019 would average out to be right about 1250 F.
Here's a useful chart to explain cone temp.
http://www.bigceramicstore.com/Informat ... Chart.html
Rob
Here's a useful chart to explain cone temp.