Page 1 of 1

Can I fix it?

Posted: Wed Jun 04, 2003 12:52 am
by Lorelei
I took some fused vases to my last show and while we were packing up one got banged against something and got a little tiny crack along the edge. Can I mend that in any way?

Posted: Wed Jun 04, 2003 1:01 am
by Brock
Not with heat. Maybe you could grind and polish it out. Brock

Posted: Wed Jun 04, 2003 1:42 am
by Martycom
Try UV glue (Optical adhesive)..... the same stuff used by dentists. I found it to be very strong, but doesn't work if the glass is purple.
Good luck.... Marty

Posted: Wed Jun 04, 2003 7:53 am
by Amy Schleif-Mohr
Marty,

I would think though that if you used the UV glue you would still see the crack. I would assume then the piece wouldn't sell.

I'm with Brock, try to grind and polish it out. Or break it into pieces and use it in something else.

Amy