when fusing two pieces of glass side by side?

Posted: Thu Jun 05, 2003 1:42 pm
by deborahbur
I fused a large platter 15x 10 and used two pieces of clear glass on the bottom (instead of one piece). When the firing was done, there was a visable line in the clear glass on the bottom. If I fired hotter would it disappear?

Thanks
Deborah

Re: when fusing two pieces of glass side by side?

Posted: Thu Jun 05, 2003 4:01 pm
by jim simmons
deborahbur wrote:I fused a large platter 15x 10 and used two pieces of clear glass on the bottom (instead of one piece). When the firing was done, there was a visable line in the clear glass on the bottom. If I fired hotter would it disappear?

Thanks
Deborah
NOPE.

Jim