Page 1 of 1

glass saw, how thin can it go?

Posted: Mon Jun 16, 2003 6:28 pm
by shasta
i'm looking for a better way to cut millefiori canes than with nippers. how thin can i slice a can using a glass saw? anyone know.

thanks.

Posted: Mon Jun 16, 2003 6:36 pm
by Brock
Under an 1/8th inch, with a good blade. Brock

Posted: Mon Jun 16, 2003 11:00 pm
by shasta
would it be easy to cut rods? not too slow?

Posted: Mon Jun 16, 2003 11:06 pm
by Brock
shasta wrote:would it be easy to cut rods? not too slow?
Very easy, but slower than nipping. You have to take some care with rod, and rotate it a few times as you cut to avoid shipping the edges. Brock

about those edges....

Posted: Wed Jun 18, 2003 4:05 pm
by Cheryl
where should she ship them to?

Posted: Wed Jun 18, 2003 4:20 pm
by Brock
The Shech Republic. Brock