Page 1 of 1

Thick BE annealing question

Posted: Fri Jun 20, 2003 10:42 pm
by Paul Tarlow
Does anyone know what BE recommends for 3/4" thick?

I have Graham's schedule -- just wondering how it compares to BE's recommendation.

- Paul

Posted: Sat Jun 21, 2003 7:50 am
by Ron Coleman
Lani has all the good stuff online these days

http://www.bullseyeconnection.com/pdfs/ ... _thick.pdf

More here, the Tech Notes are online too, bottom of the page.

http://www.bullseyeconnection.com/getsmart.html

Ron