I have a piece of fiber board that has been cut to use as a shelf in my kiln. I haven't used it yet or used the rigidizer on it. Do I need to fire it before rigidizer or just spray away and go? What temp do i need to go to and for how long?
I've finally gotten an electrician to wire up my new kiln and I'm dieing to use it but don't want to run the fiber board
Thanks for any help you can give me
Diane
HD Duraboard Fiber board
Moderators: Brad Walker, Tony Smith
-
Amy Schleif-Mohr
- Posts: 280
- Joined: Sun Mar 09, 2003 5:18 pm
- Location: Milwaukee
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
Re: HD Duraboard Fiber board
Hi DianeDiane wrote:I have a piece of fiber board that has been cut to use as a shelf in my kiln. I haven't used it yet or used the rigidizer on it. Do I need to fire it before rigidizer or just spray away and go? What temp do i need to go to and for how long?
I've finally gotten an electrician to wire up my new kiln and I'm dieing to use it but don't want to run the fiber board
Thanks for any help you can give me
Diane
I use an HD board as a shelf in my Evenheat. I use it as is, no rigidizer, no kiln wash. I have fired straight on it, no problems. But, the finish on the bottom it leaves is a bit rough, so I usually use thinfire.
I'm not sure I understand the rationale of using rigidizer, maybe someone can enlighten me?
About burnout, I recently talked to holly at Denver Kilns about a new kiln that uses HD board as a shelf and she suggested burning the board out by going 600dph to 600, hold for an hour, then go 600 dph to 1200, hold for an hour.
Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
-
Amy Schleif-Mohr
- Posts: 280
- Joined: Sun Mar 09, 2003 5:18 pm
- Location: Milwaukee
I ridgidize my fiber boards for a couple of reasons. First is to make them a bit more durable. I'm kinda rough on my shelves cause I have to dam my work so much with bricks that ridgidizing helps the life of the shelf a bit. I also fire to high temps. so it helps here too.
When I burn out a shelf I go say AFAP to 1500F.
Amy
When I burn out a shelf I go say AFAP to 1500F.
Amy
Re: HD Duraboard Fiber board
I don't rigidize either; & use regular fiber paper w/dry kiln wash sifted and smoothed with a dry haik brush - some texture yet smooth.Lisa Allen wrote:About burnout, I recently talked to holly at Denver Kilns about a new kiln that uses HD board as a shelf and she suggested burning the board out by going 600dph to 600, hold for an hour, then go 600 dph to 1200, hold for an hour.Diane wrote:I have a piece of fiber board that has been cut to use as a shelf in my kiln. I haven't used it yet or used the rigidizer on it. Do I need to fire it before rigidizer or just spray away and go? What temp do i need to go to and for how long?
I've finally gotten an electrician to wire up my new kiln and I'm dieing to use it but don't want to run the fiber board
Thanks for any help you can give me
Diane
Lisa
I can see the hold at 600F - that's where the most smoke/fumes seem to be.
Don't forget to vent!
Happy big cooking, Diane!
Jo
Thanks for the info guys. I got ahold of Marty at CDV this afternoon and he said I should lightly sand the board then fire the at 500dph to 1450 hold 15 and off.
then spray the board and fire again with the same schedule. He said this will make it smoother and stronger.
I can't wait to finally play with my HOT new friend "Kenny"
Diane
then spray the board and fire again with the same schedule. He said this will make it smoother and stronger.
I can't wait to finally play with my HOT new friend "Kenny"
Diane
-
Phil Hoppes
- Posts: 298
- Joined: Wed Mar 12, 2003 2:20 pm
- Location: Overgaard, AZ
Rigidizing is more a safety issue first and a durability issue second. Fiberboard is not nice stuff for your lungs. Check out this web site:
http://www.unifrax.com/Products
Click on Boards, then click on Duraboard products then Duraboard HD and then click on MSDS. Read it carefully!
Using rigidizer lessens your exposure to fibers by binding them on the surface. If you use a respirator when you wash these shelves, that will help. On fiber boards you should ALWAYS use your respirator. Not for the kilnwash (many, many posts on this, kinwash is a nusance dust, not a prolonged health hazard). Fiberboard is a carcinogenin.
Your lungs.
Your choice.
I rigidize.
Phil
http://www.unifrax.com/Products
Click on Boards, then click on Duraboard products then Duraboard HD and then click on MSDS. Read it carefully!
Using rigidizer lessens your exposure to fibers by binding them on the surface. If you use a respirator when you wash these shelves, that will help. On fiber boards you should ALWAYS use your respirator. Not for the kilnwash (many, many posts on this, kinwash is a nusance dust, not a prolonged health hazard). Fiberboard is a carcinogenin.
Your lungs.
Your choice.
I rigidize.
Phil
-
Amy Schleif-Mohr
- Posts: 280
- Joined: Sun Mar 09, 2003 5:18 pm
- Location: Milwaukee