90 coe and 96 coe Q

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
rodney
Posts: 167
Joined: Mon Mar 10, 2003 12:05 pm
Location: new mexico
Contact:

90 coe and 96 coe Q

Post by rodney »

i have an opportunity to acquire a large amount of 96 coe glass, and im wondering if there is any difference the casting of 96, compared to 90

thanks for you kind assistance on this matter

rodney
Betty
Posts: 18
Joined: Mon Mar 17, 2003 5:06 pm
Location: Mechanicsville MD

advice from a beginner

Post by Betty »

Take the glass coe 96 fires cooler than the coe 90 just don't mix up the glasses and mix the coe. When they come out of my kiln they all look Gooood. I fire with both and have them in seperate places in the shop.