Phoenix wire cutter

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
watershed
Posts: 166
Joined: Wed Mar 12, 2003 1:44 am

Phoenix wire cutter

Post by watershed »

Somewhere in my few memory cells, I remember reading about something called a wire cutter. I imagined it as a kind of band saw for glass. Or maybe a jewelers saw. Can anyone help my addled brain?

Or if I'm completely off base, I want to cut through / pierce a sheet of glass. A sandblaster wouldn't give me the precision I want. Water jet might, but then I'd have to find/pay someone.

Thanks
Greg
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

You might mean a Gryphon wire saw. It can work as a normal glass saw, or you can drill a hole, fit the blade in, and cut from the inside out.
watershed
Posts: 166
Joined: Wed Mar 12, 2003 1:44 am

Post by watershed »

Ahh good, just the wrong mythical beast. Thanks

Greg