Page 1 of 1

Using Overglaze with mulitply firings?

Posted: Thu Jul 03, 2003 9:06 am
by Kim Bellis
Good Morning Everyone!

This is my first time using an overglaze. The piece I am working on will take three firings. Before the first fire I sprayed Fire Master Overglaze (gave the pieces a wonderful depth - love this stuff!). My question is will I need to spray before the next two firings? I would think not - but I am famous for being wrong!

Appreciate the help and have a fun and safe holiday
Kim

Posted: Thu Jul 03, 2003 9:24 am
by Brock
I'm not familiar with that particular overglaze, but normally, the overglaze is applied only once, in the hottest firing. Brock

Posted: Thu Jul 03, 2003 3:38 pm
by Kim Bellis
Thanks Brock!

Posted: Thu Jul 03, 2003 3:41 pm
by Kim Bellis
Thanks Brock!