big kiln -vs- little kiln

Post by ajones »

I have been quite succesfully using my paragon PMC kiln (about 8X8X8) with fiberboard shelves for small fusing for a year or so. NO failures. So I get a larger glass paragon glass kiln (13X9) with ceramic shelves. it's the same controller. using the same program or going up even slower, my glass is breaking into numerous pieces. for instance a 1X2" piece might be in 6-8 pieces. Anyone have any suggestions?
ellen abbott
Posts: 148
Joined: Tue Mar 11, 2003 12:04 pm
Location: Houston Tx
Contact:

Post by ellen abbott »

There may be a temperature differential due to proximity to the coils. What is your soak temp? What kind of glass?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

My guess is that it's the shelves. Ceramic shelves hold the heat more than fiber, and you can usually fire faster on fiber shelves than on ceramic.

How fast are you increasing the temperature?