Page 1 of 1
Dichroic Scrap Supplier
Posted: Sun Jul 13, 2003 1:19 am
by Mira
I'm looking for an inexpensive dichroic scrap supplier. I've been using COE 96 glass, and would like to stay with it if I can. Does anyone have good leads?
Thanks!
Posted: Sun Jul 13, 2003 5:17 am
by Tony Smith
Inexpensive is such a relative term.... your best bet for COE 96 scrap is to go directly to CBS Dichroic (one of the sponsors of this board - just click the link above).
They are very helpful and sell their scrap by the pound or fraction thereof. I believe it was $48/lb the last time I bought some.
Tony
Posted: Sun Jul 13, 2003 8:44 am
by camaro
I use Austin Thin Films now known by Dichro Magic, they sell scrap for $ 25.00 a lb. go to:
dicromagic.com
COE 96 scrap dichro
Posted: Sun Jul 13, 2003 9:06 pm
by Tess Farley
I recently purchased about a pound of COE 96 Scrap dichroic from Carol Fonda of Auburn, California, phone for orders 888-944-3667. There were even some patterns in it. Price was $24.00.