Can someone tell me if Animal Hide Glue (Glue chipping stuff) burns off clear (no residue) when fired to tack.

...Kelly
Kitty
Posts: 444
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Post by Kitty »

havent done it. i would assume it would not burn off cleanly, too many proteins in there to carbonize, blacken, ash. maybe just put some on a little piece of glass and fire it up, see what happens. kinda curious what you're up to ... do U care to reveal?