Sandblasted glass: turning down the "white" effect

Posted: Tue Jul 15, 2003 10:51 pm
by lohman
I showed a client a sample of glass on which I used tungsten carbide @ 180 mesh (I think it's 180). She liked it but thought it looked too "white". Will the polymer coatings discussed a few months ago tone down the "whitness"? I recall reading in the discussion that it will, is my memory correct? Any other suggestions? I'm doing ten 40" x 18" glass kitchen cabinet doors so I want to get it right. I know I'll have to do a few test samples.
Thanks

Posted: Wed Jul 16, 2003 7:18 am
by Tony Smith
You probably used silicon carbide, not tingsten carbide, and yes there are a number of coatings that can be applied such as danish oil, Rain-x and Armor-All, and they will reduce the white powder look and minimize finger prints. If the doors are cleaned with spray cleaner as you would expect, eventually the coatings will have to be re-applied.

Tony

Posted: Wed Jul 16, 2003 7:50 am
by Ron Coleman
Vari Etch Frosting Powder sold by HIS GLASSWORKS was developed to do what you want.

http://hisglassworks.com/pages/varietch.html

Ron

Posted: Wed Jul 16, 2003 5:47 pm
by lohman
Thanks Tony and Ron.