I am getting ready to fuse a 24 x 24 tile.
my client is going to use it as decoration behing a stove.

Does any one think the heat from the oven would cause it to crack? some where down the road? :cry:
is there any thing I can do to help prevent it?

Thanks for any help!
Sue

Re: Heat effecting large fused tile

Posted: Wed Jul 16, 2003 11:39 am
by Bert Weiss
AZSUE wrote:I am getting ready to fuse a 24 x 24 tile.
my client is going to use it as decoration behing a stove.

Does any one think the heat from the oven would cause it to crack? some where down the road? :cry:
is there any thing I can do to help prevent it?

Thanks for any help!
Sue
Sue

Follow the rules and it should be fine.

Re: Heat effecting large fused tile

Posted: Wed Jul 16, 2003 1:29 pm
by charlie
AZSUE wrote:I am getting ready to fuse a 24 x 24 tile.
my client is going to use it as decoration behing a stove.

Does any one think the heat from the oven would cause it to crack? some where down the road? :cry:
is there any thing I can do to help prevent it?

Thanks for any help!
Sue
no, if the glass is properly annealled. most people have drywall behind their stove. if an oven gave off enough heat. that would catch fire long before glass would have had a problem.