Vic,
I'm assuming you're still quite happy with the Hyxtal if you're still using it 20 years later.
Does it really stay clear and well bonded over a long span of time? Will exposure to sun make it yellow? Any other glitches? I'm assuming what you said about the different COE glasses would rule it out for bonding different materials such as metal to glass.
			
			
									
						
										
						From your 20 years experience....
Moderators: Brad Walker, Tony Smith
- 
				Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: From your 20 years experience....
Hear is some faq from His on on the glue stuffdavebross wrote:Vic,
I'm assuming you're still quite happy with the Hyxtal if you're still using it 20 years later.
Does it really stay clear and well bonded over a long span of time? Will exposure to sun make it yellow? Any other glitches? I'm assuming what you said about the different COE glasses would rule it out for bonding different materials such as metal to glass.
http://www.hisglassworks.com/pages/faqs.html