From your 20 years experience....
Posted: Thu Jul 17, 2003 10:58 am
Vic,
I'm assuming you're still quite happy with the Hyxtal if you're still using it 20 years later.
Does it really stay clear and well bonded over a long span of time? Will exposure to sun make it yellow? Any other glitches? I'm assuming what you said about the different COE glasses would rule it out for bonding different materials such as metal to glass.
I'm assuming you're still quite happy with the Hyxtal if you're still using it 20 years later.
Does it really stay clear and well bonded over a long span of time? Will exposure to sun make it yellow? Any other glitches? I'm assuming what you said about the different COE glasses would rule it out for bonding different materials such as metal to glass.