hellu... i read a couple of the postings about the mille maker and have ordered one to give it a try. can anyone tell me what the diameter of rod does it make? i ordered mine from arrowsomethingorother.
also what's the difference between noodles and stringers. i have never heard of noodles before is it just another companies name for a stringer?

tanks diana.
lissa
Posts: 84
Joined: Tue Jun 03, 2003 8:29 pm
Location: North Carolina
Contact:

Post by lissa »

Arrowsprings, nice folks, very helpful. Stringers are round, like you know stringers to be, noodles are flat and look like fettuccini pasta noodles. I don't know about the milli maker dimensions.