fiber paper residue between layers of glass
Moderators: Brad Walker, Tony Smith
-
Barb Wolfe
- Posts: 3
- Joined: Mon Aug 04, 2003 12:25 pm
fiber paper residue between layers of glass
I'm trying to make a picture frame. I use 1/8" fiber paper between two layers of glass. Two problems: first, it is very difficult to "dig" the paper out between the two layers of glass. Is there something that will disolve the paper? Second, there seems to be a cloudy residue left. When I slide the photo into the channel left by the paper, the clear glass isn't clear - there's a film that clouds the photo. Is there a cleaner, or am I doing something wrong?
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
are you making a big flat pocket to slide the photo in? that probably will not work. the glass picks up texture from the paper. one way to do a frame is to make just the frame and then use e-6000 or some other glue to glue it on top of the glass that will cover your picture. there are lots of ways to deal with the back. rosanna