fiber paper residue between layers of glass
Posted: Mon Aug 04, 2003 12:32 pm
I'm trying to make a picture frame. I use 1/8" fiber paper between two layers of glass. Two problems: first, it is very difficult to "dig" the paper out between the two layers of glass. Is there something that will disolve the paper? Second, there seems to be a cloudy residue left. When I slide the photo into the channel left by the paper, the clear glass isn't clear - there's a film that clouds the photo. Is there a cleaner, or am I doing something wrong?