Page 1 of 1
making holes
Posted: Thu Aug 14, 2003 11:16 am
by cheryl kumiski
i was using 1/4" grinder bits to make holes in plates so they would accept clock works. the problem being 1 bit equals 3 holes. yikes!!! and i can't figure out how to use a drill press without electrocuting myself. my kingdom for a solution!!
Posted: Thu Aug 14, 2003 11:18 am
by Brock
Ask Susan Taylor Glasgow! Brock
Posted: Thu Aug 14, 2003 11:23 am
by Barbara Muth
Cheryl, there is a lot of discuission on drilling holes and drill bits in the old archives. You might find your solution there.
Barbara
Posted: Thu Aug 14, 2003 11:52 am
by starchimes (Andrea)
Try getting your bits at
http://www.lopacki.com. The prices are good. Bits last a good while. I can usually get about 50 holes per bit.
Regards,
Andrea
Posted: Thu Aug 14, 2003 1:42 pm
by paulajane
I purchased some bits that would not work with my flexible shaft set up. So we bought a cheap $20 drill press stand at Harbor Freight Tools and then adapted it to hold a cordless battery operated a drill. To keep it going steadily we slide a tie wrap over the button because battery operated drills do not have buttons to press to keep them going continuously. It works great.
Paula
Posted: Thu Aug 14, 2003 2:09 pm
by cheryl kumiski
paulajane wrote:I purchased some bits that would not work with my flexible shaft set up. So we bought a cheap $20 drill press stand at Harbor Freight Tools and then adapted it to hold a cordless battery operated a drill. To keep it going steadily we slide a tie wrap over the button because battery operated drills do not have buttons to press to keep them going continuously. It works great.
Paula
thanks paula--this seems the most effective. i did check the archives and most of the info concerns a dremel tool. since i need a 1/4" hole drilled through 6 layers of glass the dremel isn't an option. i'll try a regular drill with diamond bits.
cheryl
Posted: Thu Aug 14, 2003 2:10 pm
by cheryl kumiski
Brock wrote:Ask Susan Taylor Glasgow! Brock
how??
Posted: Thu Aug 14, 2003 2:11 pm
by cheryl kumiski
starchimes wrote:Try getting your bits at
http://www.lopacki.com. The prices are good. Bits last a good while. I can usually get about 50 holes per bit.
Regards,
Andrea
thank you!! will do.
cheryl
Posted: Thu Aug 14, 2003 2:59 pm
by Dick Ditore
Harbor freight also sells diamond coring bits in small sizes. I have used the 1/2" and the 1". I use my bench drill press. You have to lubricate. I bought a suction ring at cr laurence, and fill with water. Go easy and no problem. I have cut up to 1 3/8" holes.
Dick
Posted: Thu Aug 14, 2003 4:15 pm
by Paul Tarlow
Brock wrote:Ask Susan Taylor Glasgow! Brock
...saw that one coming
Making holes
Posted: Mon Aug 25, 2003 1:21 pm
by Alecia Helton
Sorry to be a late reply. I just joined the list.
I bought my drill press at Home Depot, the drill was included with the press. I buy the hollow-core diamond bits from Rio Grande.
To drill with water: I place a large plastic lid on the base plate to protect the metal from from the wet sponge that lays on top of it. I use a squirt bottle to keep the drill and glass wet.
There are times when you really need three hands. And I have used my chin at times, but I've never feared electrocution.
Hope this helps.
Alecia