Page 1 of 1
How do I make a 1-piece shelf from a 3-pc. shelf?
Posted: Sat Aug 16, 2003 11:23 pm
by Pamela B.
I have a new Evenheat 2542 kiln with a three-piece shelf and would like to be able to make something larger than what each individual piece can accommodate. What is the best way to span the gap between pieces? A single sheet of fiberboard?
Pam
Posted: Sun Aug 17, 2003 12:51 am
by Lisa Allen
I have a big Evenheat as well and cut those 3 shelves up for dams. I use a Unifrax HD 1 and 1/2" duraboard as a shelf instead, sitting right on the kiln floor......works just fine.
Lisa
Posted: Sun Aug 17, 2003 10:11 pm
by Marty
ditto on kiln and solution.
Marty
Posted: Mon Aug 18, 2003 11:58 pm
by Pamela B.
Thank you thank you thank for the suggestions. Now, why doesn't Evenheat suggest this solution? Or the distributor from whom I bought the kiln? What's the point to having a 3-piece shelf if one wants to make one big thing? Or, as was my intention, to make four 14" plates? Grrr.
Posted: Tue Aug 19, 2003 8:07 am
by Marty
Don't forget to rigidize the board.