Page 1 of 1
Looking for Special Slumping mold and need help
Posted: Tue Aug 19, 2003 6:22 pm
by Ernsglass
I am looking for an elongated (maybe even considered oval) mold for slumping. The one I am looking for is about 16 inches long and maybe 5 inches or so wide at the largest part. I is kind of oval in shape but not a true oval. I have heard it referred to as a "bread" server shape. If you were to elongate an oval that is what I am looking for. I have searched the web with no luck. I have heard there is a place in North Carolina or Tennessee but again have had no luck. Would apprecaite any leads or help. Thanks in advance.
Posted: Tue Aug 19, 2003 11:01 pm
by Lisa Allen
Posted: Tue Aug 19, 2003 11:15 pm
by Ron Coleman
Try this link
http://www.cdvkiln.com/menufusingsupplies.htm
Look on the left side of the page and click on "molds"
Look at the list of molds, the long and short OVAL molds (#8951 and #8952) are close to what you're looking for.
Ron
Posted: Wed Aug 20, 2003 10:42 am
by Stephie
Have you tried your local ceramics store? They usally have every shape and size.
Steph
Posted: Wed Aug 20, 2003 3:01 pm
by John
I got one from a local ceramic supplier.
John
bread mold..very long
Posted: Thu Aug 21, 2003 1:54 am
by doc
Posted: Fri Aug 22, 2003 12:49 am
by Lionel
Select an oval shape that is close to what you want and cut your glass short. You will end up with a liped bread board shape. - OR