Page 1 of 1

Fine Silver and BE White

Posted: Sun Aug 24, 2003 9:38 am
by Melissa Terman
I am working on a project with a very tight deadline. Has anyone used Fine Silver as an inclusion or next to Bulls Eye White? Does the white react oddly to the silver like the French Vanilla does?

As always, thank you for sharing your experience.

Posted: Sun Aug 24, 2003 12:57 pm
by Lou_Ohio
I have used this combination ( opal white & Fine silver ) without a problem .

Lou

Posted: Sun Aug 24, 2003 1:25 pm
by Dani
How do you prevent silverstain (yellow halo-ing)? Thanks.