Page 1 of 1
Glass Slumping Groups in Texas
Posted: Wed Aug 27, 2003 3:55 pm
by southwest-designs
We are interested in finding glass slumping groups in Texas. San Antonio area would be preferable. We are new to the art form and would like to take classes or participate in work shops.
Posted: Wed Aug 27, 2003 4:23 pm
by starchimes (Andrea)
You might try asking the folks at
http://www.aaproducts.com. They are located in Seguin which is pretty close I think.
Posted: Wed Aug 27, 2003 6:10 pm
by vblue
Paul Tarlow in Austin teaches a lot of classes.
We have classes but we are in Fort Worth. Before Paul started teaching classes, we had people drive up for our classes. Maybe you can contact him, his work is terrific.
We don't have the current classes listed yet on the website but you can see what we offer on the website:
http://www.merry-go-roundstainedglass.com
We are having a fusing class in Oct. and a slumping class in Nov. and also do private classes.
Vernelle
Posted: Wed Aug 27, 2003 9:41 pm
by LesleyNolan
Linda Hirsch is a glass fuser in San Antonio, Texas. She has about 12 years experience and a lot of fun as well. You can contact her through her email address
lhirsh@satrx.rr.com
If you have trouble reaching her let me know. You can email me at
Lesley@LesleyNolanGlass.com
Thanks!
Posted: Wed Aug 27, 2003 11:41 pm
by southwest-designs
Thanks to everyone for your replies. They will be most helpful.
Posted: Thu Aug 28, 2003 1:27 pm
by Susan Wright
Check with Dianes Rainbow of Glass Shop. Think that's the name. They have fusing and lampwork along with traditional stained glass classes.
Susan W
Posted: Mon Sep 01, 2003 12:31 am
by Paul Tarlow
vblue wrote:Paul Tarlow in Austin teaches a lot of classes.
We have classes but we are in Fort Worth. Before Paul started teaching classes, we had people drive up for our classes. Maybe you can contact him, his work is terrific.
We don't have the current classes listed yet on the website but you can see what we offer on the website:
http://www.merry-go-roundstainedglass.com
We are having a fusing class in Oct. and a slumping class in Nov. and also do private classes.
Vernelle
Actually, I teach somewhat infrequently (my next class is a Frits and Powders class in early November). The Art Glass Fusing Center (
http://www.glassfusingcenter.com) in north Austin (up 183)where I teach does have lots of classes at a variety of levels. Also, Blue Moon (on N. Lamar near Northloop) teaches some fusing classes (
http://www.austinbluemoon.com).
Thanks for the kind words Vernelle. One of these days I hope to get up to Ft. Worth and see you all.
- Paul