Adjusting Your Chicago Tile Saw Part Two
Posted: Thu Aug 28, 2003 4:06 pm
With the saw still unplugged and the guard off, place the square flat on the table as shown and LIGHTLY against the blade.

If it needs adjusting, loosen the two large bolts at each end of the machine
then loosen the allen screws and move the bar side to side at both ends until it's square. First tighten the allen screws, THEN the two large bolts. Then check for squareness. Repeat if necessary.

Randy
If it needs adjusting, loosen the two large bolts at each end of the machine
then loosen the allen screws and move the bar side to side at both ends until it's square. First tighten the allen screws, THEN the two large bolts. Then check for squareness. Repeat if necessary.
Randy