I need to remove liver of sulfur patina on silver foil. Can someone tell me at what temps. it will burn off.

Thanks ...K
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

By 1000f
My memory is so good, I can't remember the last time I forgot something . . .
KellyG
Posts: 67
Joined: Sun Mar 09, 2003 11:12 pm
Location: Baton Rouge, LA
Contact:

Post by KellyG »

Thanks Brock. It was 850 in my kiln. Your answer surprised me tho. I thought it would have been below 500. Glad I posted and you answered.