Photosensitive Glass

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
gone

Photosensitive Glass

Post by gone »

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Post by Tony Smith »

Kewl

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
PDXBarbara
Posts: 292
Joined: Sun Mar 09, 2003 4:09 pm
Location: Portland, OR

Post by PDXBarbara »

Went to the demo put on by Olympic Color Rods during GAS....John Leggot (Gaffer Glass) led the demo at Chihuly's boathouse studio. The photosensitive currently only comes in rods. but there was talk of sheet too, down the road. Rod (Gaffer Ruby) is $70/kg. (2.2lb/kg). They also have Reichenbach photosensitive glass....rods only...
yellow is $46/kg; gold ruby $43 ; copper ruby (not priced).


Yo Els! How was Boise?
Barbara
Barbara Bader