After months of research ,obcessing ,and talking with makers of many kilns I ordered a custom kiln from olympic.I have not heard anyone speak of Olympic.but they were the only makers willing to work with me.
Specs:
30x42x27.
I do mostly casting, so I needed deep. But I want to do fusing in future. So it will have elements in lid,that can be used alone or shut off, a method to cut off power when open, a glass port hole at top. kiln sitterfor manual use , three zone control, and a glass controller on wall. Plus a counter weight system that will be mounted onto the three ring  kiln in my basement so that entry into basement will be possible.
It was to be shipped this week, but double checking my order I found that they were making it 18" Deep intead of 27" So they will make this change first. Cynthia and Bob Haugen are the owners and they have been very helpful. I will let you know how it works out. The kiln I have been using is 3 ring Skutt  octagon shape  kiln I bought in1974. I love it and am going to have it rewired.and bricks replaced.
I use digitry with this one. It has been down for three months.I am taking this oportunity to make a good,safe shop in my basement but 'jonsing' for
the creative flow.
Judi  