Page 1 of 1
Large Kiln shelves- where can I buy one?
Posted: Mon Sep 29, 2003 4:11 pm
by karla
Does anyone know where I can purchase a kiln shelf larger than 20" x 20"? My kiln is can accomodate 20"W x 38"L; ideally, I would like somehting 20"W x 28" (up to 38") long....thanks!
Posted: Mon Sep 29, 2003 4:21 pm
by Barbara Muth
Karla, are you looking for a mullite shelf or a fiber shelf?
large kiln shelves
Posted: Mon Sep 29, 2003 5:17 pm
by karla
I am looking for the regular ceramic type; if that is mullite, then that is what I want....
Posted: Mon Sep 29, 2003 5:29 pm
by Barbara Muth
I don't think mullite shelves come bigger than 20 by 20. Bigger would be too heav. You would need 2 people to put in and take out your shelf. That's why many people are using shelves made of fiberboard. Not sure where you would get them, but plenty of people here do know.