Hi all.
Has anyone used the braided fiber robe? What is it good for. A dam to keep round pieces shape and thickness??
Thanks Lisa W
[/img]
-
Brock
- Posts: 1519
- Joined: Mon Mar 10, 2003 1:32 pm
- Location: Vancouver, B.C.
Post
by Brock »
It's usually used as a gasket to prevent heat loss, around kiln lids, for instance. As a robe, it's too scratchy! Brock