Page 1 of 1
					
				fusing riverstones with glass
				Posted: Sat Oct 04, 2003 11:17 am
				by Paulette
				Can one successfully fuse river stone (small) with glass?
Thanks for your answers...and all the info you give on this board!
Paulette
			 
			
					
				Re: fusing riverstones with glass
				Posted: Sat Oct 04, 2003 11:34 am
				by Brock
				Paulette wrote:Can one successfully fuse river stone (small) with glass?
Thanks for your answers...and all the info you give on this board!
Paulette
No, you can't. You can combine rocks or stones with slumped glass, but not fused together. You could make a mold of the stones, slump the glass over the mold, then glue the rocks into the depressions.  Brock
 
			 
			
					
				
				Posted: Sat Oct 04, 2003 3:49 pm
				by Barbara Cashman
				I remember a long thread about this that should be in the archives.  Good luck. - Barbara