Page 1 of 1
					
				Glass cabinet knobs/pulls and other things...
				Posted: Mon Oct 06, 2003 2:15 pm
				by Joanne in QB
				A few questions here: 
1. Where can one purchase the knobs and pulls for cabinets that do not already have a decorative face?
2. How do you attach the glass piece securely?
3. Do any of you have a polarimeter or sheet of polaroid film? Or, how do you know for sure your piece won't fracture down the road. I have heard of situations where a piece falls apart 3 years down the road, even though it was 'compatible' glass, etc., etc. Where would one get these items? Am I paranoid or would it be a good quality control to use them to ensure the final product is stable?
Thanks everyone.
			 
			
					
				
				Posted: Mon Oct 06, 2003 2:19 pm
				by charlie
				1: home supply store, one step up from a home depot type place. just look for standard knobs with a flat face.
2: epoxy
3: a pair of cheap polorized sunglasses. disassemble and use the 2 lenses.
			 
			
					
				
				Posted: Tue Oct 07, 2003 8:13 am
				by Tom White
				Two sources for polarizing film are American Science and Surplus, 
http://www.sciplus.com/   and Edmund Scientific, 
http://scientificsonline.com/default.asp?
Best wishes, 
Tom in Texas
 
			 
			
					
				please delete
				Posted: Tue Oct 07, 2003 9:51 am
				by Bert Weiss
				please delete
			 
			
					
				Re: Glass cabinet knobs/pulls and other things...
				Posted: Tue Oct 07, 2003 9:53 am
				by Bert Weiss
				Joanne in QB wrote:A few questions here: 
1. Where can one purchase the knobs and pulls for cabinets that do not already have a decorative face?
2. How do you attach the glass piece securely?
3. Do any of you have a polarimeter or sheet of polaroid film? Or, how do you know for sure your piece won't fracture down the road. I have heard of situations where a piece falls apart 3 years down the road, even though it was 'compatible' glass, etc., etc. Where would one get these items? Am I paranoid or would it be a good quality control to use them to ensure the final product is stable?
Thanks everyone.
Joanne
I got stainless steel cabinet pulls that are cylindrical with a flat face from Lee Valley Tools.  They have warehouses in Canada and USA. I have not yet glued my glass to them, but I will probably use an epoxy like PC7 or maybe Gorilla Glue.  My glass is black BE so is opaque. If your glass is transparent, use any glue designed to hold a rear view mirror on to a windshield.  UV glues are good for this.
Being sure about your process is a tricky affair.  The polarizer will help you understand how you are doing when using a base of clear glass.  You have to extrapolate over to colored glasses.
Personally I like the dishwasher test.  If it survives in your dishwasher, the rest of life will be a piece of cake.
Edmund Scientific sells a sheet of polarized film for $20. Cut it in half.
 
			 
			
					
				
				Posted: Tue Oct 07, 2003 1:45 pm
				by Lisa W.
				Joanne,
I did all the pulls for my cabinets and they are solid.
I used a plastic or lexan pulls for the backing. Not sure where I got them I will hunt it up. They where ment to be used as is so I sliced then thinner and for the knobs I just cut them shorter. I. used E600 industrial glue.
Hope this helps. Lisa w