Screen Printing setup Pictures
Posted: Sun Mar 23, 2003 10:29 pm
I uploaded some pictures of my screen printing setup to the web. This is how my maglesses were done.
The base is particle board with oak trim and Formica top. The hinges are from Dick Blick Art Supplies.
Cardboard strips help position the glass. The silkscreen frame is 18" x 20" from Pocono Screen. The photo emulsion is Ulano CDF-QT50.
Ron
http://mrcol.freeyellow.com/screen-printing/