Schedules for Murano (Effetre)?
Posted: Mon Oct 13, 2003 7:17 am
I've got some Murano sheet and millefiori, coe 104.
I'm firing 2 layers sheet + millifiofi + bits of cut sheet. Sheet colours clear + turquoise transp + translucent white. (max 11cm square)
I've done compatability tests to 800 (deg C), anneal 30 min at 520, and all seems OK - this gave a 'full but not flat' fuse.
I want to fuse flat (I tried 836, Bullseye full fuse) but this was too hot and the glass flowed out.
Anyone have a schedule for a full flat fuse, also for a shallow slump?
(working with a front loading kiln, shelf size 45 x 30 cm)
I'm firing 2 layers sheet + millifiofi + bits of cut sheet. Sheet colours clear + turquoise transp + translucent white. (max 11cm square)
I've done compatability tests to 800 (deg C), anneal 30 min at 520, and all seems OK - this gave a 'full but not flat' fuse.
I want to fuse flat (I tried 836, Bullseye full fuse) but this was too hot and the glass flowed out.
Anyone have a schedule for a full flat fuse, also for a shallow slump?
(working with a front loading kiln, shelf size 45 x 30 cm)