:?: I have been making cheese boards from wine bottles, I now have some one who would like a red wine bottle and a purple one, there are none of these around .I was wondering if I could coat the insde of the bottle with a glass paint and then put it into the kiln, what paint would be the best and can I do it a about 1480 to 1510 d , I hope someone might have an idea, thanks Andy

Posted: Wed Oct 22, 2003 9:44 pm
by Tom White
You might want to look at Unique Glass Colors, http://uniqueglasscolors.com/glaslf.html