Page 1 of 1
Pre Cut Circles?
Posted: Tue Oct 28, 2003 12:08 am
by daffodildeb
Does anyone sell 90 or 96 COE circles in small diameters--say 1" to 2" or so? I'd like to buy a number of them in either clear or colored glass.
Posted: Wed Oct 29, 2003 2:49 am
by Lynne Chappell
Not as far as I know.
Posted: Wed Oct 29, 2003 7:54 am
by amy carew-sturgis
My mom sent me a link to a rubber stamping website
http://www.stampington.com that sells glass circles. They appear to be pre-fired with a hole in the top to make charms out of. Not sure if this is what your looking for, but it might help.
-Amy
small circles
Posted: Wed Oct 29, 2003 8:36 am
by scooter riegelsperger
Deb,
I can make 'em. any size. your scrap or mine. I'm in Houston. Call me.
713-562-0426.
Scooter
Posted: Wed Oct 29, 2003 5:09 pm
by Harry
We cut and sell circles and other standard and custom shapes. Prices for circles including glass (Bullseye clear 3mm) 1"-27cents each; 1.5"- 40 cents; 2"-58 cents, 2.5"-85 cents. Colors slightly more. We need to sell them in multiples that can be cut from a full sheet (ie 1" in multiples of 60 and 2"in multiples of 32). Call about colors other glass etc.
Water Jet Design Hillsboro OR 503-615-0144