Post by Deb Lewis »

Not nearly as experienced as you guys, but when I was having problems with flairs after years of no problems it was my breaking pliers. I'll often use them to pull off strips. When I checked the edge of the jaws they were concave. New ones did the trick.

Just in case you're using breaker/grozers.