Page 1 of 1
					
				kiln wash on kiln floor?
				Posted: Thu Oct 30, 2003 3:22 pm
				by Michelle Fokos
				hi,
thanks to input from Brock, Avery and Barb awhile back i have finally chosen to get a skutt clamshell, and have an electician coming tomorrow to put in my 240 outlet for it!! 
i've heard from many folks that it is a  good idea to paint the floor of the kiln with kiln wash, but spoke with Neil at Skutt the other day and he disagrees.  he feels that coating the floor with kiln wash changes the thermodynamics of the kiln in a negative way.  wondering what any of you think about this...
thanks so much,
michelle
			 
			
					
				
				Posted: Thu Oct 30, 2003 3:48 pm
				by Tony Serviente
				Whats the lining for the clamshell?
			 
			
					
				
				Posted: Thu Oct 30, 2003 3:54 pm
				by Amy on Salt Spring
				I'm no expert in thermodynamics but I can't imagine how a couple of thin coats of kiln wash could have any affect whatsoever on heat distribution in a kiln.  What it does do is make any accidents or pieces that roll off the shelf an easy clean up instead of a permanent part of the kiln.  I can't count the number of times I've had some doodah slip out of my tweezers and roll off the shelf and under.  If I had to take the whole shelf out to get it--well it would be a huge pain.  I would think a large buildup of stuck glass would be more likely to change thermodynamics!
Amy
			 
			
					
				Re: kiln wash on kiln floor?
				Posted: Thu Oct 30, 2003 4:18 pm
				by Brad Walker
				michelle f wrote:i've heard from many folks that it is a  good idea to paint the floor of the kiln with kiln wash, but spoke with Neil at Skutt the other day and he disagrees.  he feels that coating the floor with kiln wash changes the thermodynamics of the kiln in a negative way.  wondering what any of you think about this...
One of those "many folks" you may have heard of regarding kiln washing the floor of the kiln is Skutt.  The operating manual for their glass kilns recommends that after you kiln wash the shelves "you may also want to coat the floor of the kiln."  This is from page 7 of the manual: 
http://www.skutt.com/glass/resources/op_man.php
The do strongly 
(bold print!) tell you to never kiln wash the walls or the lid of the kiln.  I wonder if that's what Neil was referring to.
As for me, I think kiln washing the floor makes good sense.  You don't have to do it often, but if powder or frit ever spills on the floor (and it will!) you'll be grateful.
 
			 
			
					
				
				Posted: Thu Oct 30, 2003 5:34 pm
				by Mira
				My kiln floor is washed - my glass melts just fine.
 
 
			 
			
					
				
				Posted: Thu Oct 30, 2003 6:08 pm
				by PaulS
				I sift plaster on the floor (with a liberated flour sieve) and vaccuum it out with a mini car-vac every couple of firings and then sift some more.
Plaster is cheaper than kiln wash, that's all.
			 
			
					
				
				Posted: Thu Oct 30, 2003 6:27 pm
				by Amy on Salt Spring
				Do you worry that little motes of plaster dust will float around and get into the glass?  I put kiln wash, maybe four thin layers, on the floor of my kiln two years ago and have never recoated and it works just fine still.  No need to vacuum up anything or redo anything.  Its BE kilnwash--works great and almost no expense whatsoever.
Amy
			 
			
					
				
				Posted: Thu Oct 30, 2003 6:28 pm
				by Brad Walker
				Paul Stevenson wrote:I sift plaster on the floor (with a liberated flour sieve) and vaccuum it out with a mini car-vac every couple of firings and then sift some more.
Plaster is cheaper than kiln wash, that's all.
Not really.  I kiln wash the floor, then forget it.  No need to ever re-apply unless you have a disaster.
 
			 
			
					
				
				Posted: Thu Oct 30, 2003 6:29 pm
				by charlie
				if you use wash, you only have to do it once until you have a major spill. i haven't redone mine since i got it, almost 2 years ago.
			 
			
					
				
				Posted: Thu Oct 30, 2003 6:56 pm
				by Stephie
				You all have me thinking.  My kiln is a used ceramic kiln.  It looks like it had been previously washed, but should I add to it?  You don't have to remove the old do you?  If so how?  Is there a difference between ceramic & glass kiln wash (in regards to the bottom of the kiln only)?
Thanks - Steph
			 
			
					
				
				Posted: Thu Oct 30, 2003 7:11 pm
				by charlie
				can you see the kiln floor through holes in the wash? it never hurts to recoat, but it may not be necessary. a couple of minutes and a few cents of wash won't break you.
no you don't remove old wash, and there no practical difference in washes except glass wash is usually ground more finely.
			 
			
					
				
				Posted: Thu Oct 30, 2003 7:36 pm
				by Stephie
				Thanks Charlie.  There are crack between the brick, cheep insurance.
			 
			
					
				Re: kiln wash on kiln floor?
				Posted: Thu Oct 30, 2003 7:42 pm
				by Cynthia
				michelle f wrote:...i've heard from many folks that it is a  good idea to paint the floor of the kiln with kiln wash, but spoke with Neil at Skutt the other day and he disagrees.  he feels that coating the floor with kiln wash changes the thermodynamics of the kiln in a negative way.  wondering what any of you think about this...
thanks so much,
michelle
What is the floor of this kiln made of,  fire brick, fiber board? Glass can erode through brick or RCF materials over time. I would wash it regardless to protect the floor of the kiln.  It's possible it might change the thermodynamics somewhat, but the kiln isn't so big that it would be significant (this kiln has a 20" shelf right?), but that's just a hunch on my part.
 
			 
			
					
				
				Posted: Thu Oct 30, 2003 9:14 pm
				by jerry flanary
				'Tis better to have washed and lost than never to have washed at all.
			 
			
					
				KIln wash on bottom
				Posted: Thu Oct 30, 2003 11:38 pm
				by Judi Charlson
				I kiln washed the bottom of my new kin leaving an inch boarder from sides. I was told a long time ago that  Kiln wash should never come in contact with elements
In my old ceramic Skutt kin I always placed a layer of course grog on the bottom. any spills collected on that. I always used grog under ceramic sculptures when firing on shelves to let the sculpture move around a bit to prevent cracks or to  level it. I also use grog under plaster molds to level and also think it alows for it to move slightly without friction. It also protects any frit from falling on shelf if I  fill the mold after it is in kiln.I really don't know where I got that idea or if it really helps. 
Judi
			 
			
					
				Re: kiln wash on kiln floor?
				Posted: Thu Oct 30, 2003 11:51 pm
				by dee
				michelle f wrote:hi,
thanks to input from Brock, Avery and Barb awhile back i have finally chosen to get a skutt clamshell, and have an electician coming tomorrow to put in my 240 outlet for it!! 
i've heard from many folks that it is a  good idea to paint the floor of the kiln with kiln wash, but spoke with Neil at Skutt the other day and he disagrees.  he feels that coating the floor with kiln wash changes the thermodynamics of the kiln in a negative way.  wondering what any of you think about this...
thanks so much,
michelle
having just opened the kiln to see the results of this morning's firing, i have the perfect example of why one applies kiln wash to the floor of the kiln ;P the base piece of glass did something unexpected and some of it is down the side of the shelf and puddled on the floor ;P ah well, some of it will become cabs ;P some will go in the recycle bin ;P apparently the kiln goddess felt like playing in my kiln today ;P
D
 
			 
			
					
				kiln wash on floor
				Posted: Fri Oct 31, 2003 12:17 am
				by slats
				I kiled washed the floor when my kiln was new.  Recently I raked and glass spilled onto floor....When I removed the warm cabs from the floor the next day some of the brick floor came off with the cabs leaving indentations in the brick.....So upsetting....Should I reapply washto those areas?
			 
			
					
				
				Posted: Fri Oct 31, 2003 11:00 am
				by jerry flanary
				hell yes.
			 
			
					
				Washing the floor
				Posted: Fri Oct 31, 2003 2:29 pm
				by Jerry
				Some time back I did a 14" round combed piece which I didn't keep an eye on, and it grew to OVER 20".  I say "over" because that's the size of my shelf and it was off the shelf on three sides.  I recoated the floor with new wash after that and never looked back, but I do pay a little more attention.
Jerry
			 
			
					
				
				Posted: Fri Oct 31, 2003 3:07 pm
				by Michelle Fokos
				thanks for all the replies!
the floor of the clamshell is fire brick, and i am going to coat it with kiln wash.  the person i spoke with at skutt was aware that the manual recommended this process, but he was in disagreement with it.  but it sounds like a very tried and true method to me.  
the electrician is here right now putting in my new outlet!! yippee!!
thanks again,