Re: Bowl made with frozen frit
Posted: Sat Jan 05, 2008 4:57 pm
I'm not sure I do need to freeze, Raf, but in the other freeze & fuse discussions people were talking about freezing with CMC/water binder in order to get more workability from it before firing. Maybe I misread the posts! I'll go check again.
D.