Re: What's the fastest you'll cool glass?
Posted: Wed Jan 09, 2008 11:50 am
Thanks for your thorough response, Joseph! Quite helpful.Joseph Tracy wrote: 1300 sounds a little high for enamels. Is that the recommended temp? Maybe they are lead free? What brand?
To answer your question, the enamels in question are Fusemaster high-fire opaques. I used to only prefire them to 1100, as I would do with glass stainers colors and low-fire enamels, but at that temp they're not fully baked and when capped and fused the images smear.