Posted: Sun Feb 17, 2008 8:59 pm
by Pam
Has anyone tried putting a kiln shelf on top of a disk to be dropped through a drop ring in order to prevent it from falling through? Any other thoughts on keeping the disk from falling through?
Thanks,
Pam
Re: drop ring question
Posted: Sun Feb 17, 2008 9:01 pm
by Jennifer Polver
What is your schedule? All my drop ring disasters have been a result of my schedule
Re: drop ring question
Posted: Sun Feb 17, 2008 9:09 pm
by Pam
Typically I've been going at 300 dph to 1100 then 25 dph to 1250 and holding until it's done. This is for BE 3 - 4 layers. The one yesterday was a bit smaller than the outer edge of the dropring so I was worried from the start.
Pam