i am firing half inch thick pattern bar strips butted together and I am getting some sinkholes in some places where the seams are, primarily in the transparent colored areas. I am thinking that I am not firing hot enough and if I increase the temp, the surface will level out. I only went to 1450 and am thinking that I will leave it dammed and go up again but to 1500 this time. Anybody got any thoughts?
Thanks Lisa
sinkhole question
Moderators: Brad Walker, Tony Smith
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
sinkhole question
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
So upping the temp will work.......thanks. Now, I used thinfire under the slices and I would like to just refire as is, leaving the dams, the paper and the 1/8" paper dam liners. Any problems with that? Do I need to pull it out and put new thinfire?
thanks, Lisa
thanks, Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact:
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
Thanks, Tony. It is recooking now going up 150dph. Hope that is slow enough.......guess I'll see tomorrow.
Lisa
Lisa